當前位置:首頁 > 新聞中心 > 保定環氧地坪施工后的“雀斑”怎么辦?解決方法

保定環氧地坪施工后的“雀斑”怎么辦?解決方法

2021-12-21

保定環氧地坪的出現改變了很多工廠的車間環境,保定環氧地坪漆是現在比較環保使用的一種地面漆。在對于保定環氧地坪的使用中我們還有需要了解的地方,在河南保定環氧地坪漆的施工后的一些問題是我們需要關注的,在施工后比較突出的問題就是在涂膜的表面上會出現局部的收縮,而形成麻麻點點。這樣的情況要怎么處理呢?下面我們就一起來了解一下。

The appearance of epoxy floor has changed the workshop environment of many factories. Epoxy floor paint is a kind of floor paint which is used more environmentally. In the use of epoxy floor, we still need to understand the place, in Henan epoxy floor paint after the construction of some problems we need to pay attention to, after the construction of the more prominent problem is that there will be local shrinkage on the surface of the film, and the formation of pockmarks. How do we deal with such a situation? Now lets look at it together. 原因一:保定環氧地坪漆涂料中硅油類的低表面活性的助劑加入量過多。

Reason 1: the low surface active additives of silicone oil in epoxy floor paint are too high.

解決方法:應控制硅油等表面活性劑的加入量。

Solution: we should control the amount of silicone oil and other surfactants.

原因二:溶劑或稀釋劑中所含低沸點、高沸點的溶劑過多,而且配比也不合適。

Reason 2: Solvents or diluents contain too many solvents with low boiling point and high boiling point, and the ratio is not appropriate.

解決方法: 應注意低沸點、高沸點溶劑的使用量和各種沸點溶劑的配比。

Solution: attention should be paid to the usage of low boiling point, high boiling point solvent and various boiling point solvents.

原因三:被涂物表面的油垢、蠟質、金屬皂類和潮氣等未除凈。被漆物表面留有殘酸、殘堿 。

Reason three: grease, wax, metal soap and moisture on the surface of the coating are not removed. Residual acid and alkali residue on the surface of the paint.

解決方法:被涂物表面的油垢、蠟質、金屬皂類、殘酸、殘堿和潮氣等在保定環氧地坪漆施工前應處理干凈。

Solution: The grease scale, wax, metal soap, residual acid, residual alkali and moisture on the surface of the coating should be cleaned before the application of epoxy floor paint.

原因四:噴涂施工中帶入油或水,噴槍和物面間距離太近。

Reason four: spraying oil or water into the construction process, the distance between the spray gun and the material surface is too close.

解決方法:保定環氧地坪施工前應檢查噴漆機器的油水分離器是否正常,應掌握好噴槍和物面間的距離。

Solution: Before the construction of epoxy floor, the oil-water separator of the spray painting machine should be checked whether it is normal or not, and the distance between the spray gun and the object surface should be well controlled.

原因五:噴槍噴嘴口徑太小,而噴漆壓力又過大。

Reason five: the nozzle size of the spray gun is too small, and the spray paint pressure is too large.

解決方法:選擇好噴槍的口徑和噴涂壓力。

Solution: selec the caliber and spray pressure of the spray gun.

原因六:噴涂河南環氧保定環氧地坪施工中涂料粘度過低或過高。

Reason six: paint viscosity in Henan epoxy floor construction is too low or too high.

解決方法:掌握好合適的施工粘度。

Solution: grasp the proper construction viscosity.

原因七:溶劑揮發得太快,涂膜還來不及流平。

Reason seven: solvents evaporate too fast, and the film is too late for leveling.

解決方法: 不能選用揮發性太強的溶劑施工。

Solution: do not choose too strong solvent for construction.